I apologize ahead of time if all of you have covered this in the past. I am a newbie to the forums here :oops: .

I emailed Tyler about this recently and he was kind enough to offer some info and advice. I would like to get input from the forum on whether you pre-carb your bowls, and if so, what is your favorite recipe or technique.

Thanks!
Steve Shawl
User avatar
KurtHuhn
Site Admin
Posts: 5326
Joined: Thu Nov 23, 2006 8:00 pm
Location: United States/Rhode Island

Post by KurtHuhn »

I precarb everything unless a customer requests a pipe without. I've only had one request in something like 4 years of selling my pipes.

I use the waterglass, pumice, and charcoal recipe.
Kurt Huhn
AKA: Oversized Ostrogoth
artisan@k-huhn.com
sshawl
Posts: 16
Joined: Sun Aug 26, 2007 11:10 pm

Post by sshawl »

Thanks Kurt. I appreciate the reply. Could you offer a bit more detail on the recipe? :D

Steve
User avatar
bvartist
Posts: 463
Joined: Thu Nov 23, 2006 8:00 pm
Location: United States /Missouri
Contact:

Post by bvartist »

I precarb all my pipes unless someone asks for one without the precarb. I use the buttermilk/sour cream/charcoal recipe. About half and half buttermilk/sour cream then enough charcoal to make it black.
User avatar
KurtHuhn
Site Admin
Posts: 5326
Joined: Thu Nov 23, 2006 8:00 pm
Location: United States/Rhode Island

Post by KurtHuhn »

sshawl wrote:Thanks Kurt. I appreciate the reply. Could you offer a bit more detail on the recipe?
It's a mix of pumice and activated charcoal in roughly equal amounts, and enough waterglass to make it roughly the consistency of latex interior paint. I know some folks keep a container of this stuff around and just ad to it as it gets low, but mine seems to harden up on me before too long, so I just mix a small amount when I have a batch of pipes ready to be coated.
Kurt Huhn
AKA: Oversized Ostrogoth
artisan@k-huhn.com
User avatar
hazmat
Posts: 797
Joined: Thu Nov 23, 2006 8:00 pm
Location: Harrisburg, PA

Post by hazmat »

Where does one find waterglass? I know what it is, just not where to find it.
User avatar
RadDavis
Posts: 2693
Joined: Thu Nov 23, 2006 8:00 pm
Location: united states/Alabama
Contact:

Post by RadDavis »

Waterglass can be found at an old time drug store. Usually the family owned kind that has been around forever.

Rad
User avatar
hazmat
Posts: 797
Joined: Thu Nov 23, 2006 8:00 pm
Location: Harrisburg, PA

Post by hazmat »

Thanks Rad.. unfortunately there's none such in my area. It's all Rite-Aids and CVS's round these parts. Any ideas where it can be gotten on the web?
User avatar
RadDavis
Posts: 2693
Joined: Thu Nov 23, 2006 8:00 pm
Location: united states/Alabama
Contact:

Post by RadDavis »

User avatar
bvartist
Posts: 463
Joined: Thu Nov 23, 2006 8:00 pm
Location: United States /Missouri
Contact:

Post by bvartist »

Out of curiosity.......why use pumice? I'm guessing it adds additional roughness to the coating when it is dried. Or is it something necessary in the waterglass recipe?
User avatar
KurtHuhn
Site Admin
Posts: 5326
Joined: Thu Nov 23, 2006 8:00 pm
Location: United States/Rhode Island

Post by KurtHuhn »

hazmat wrote:Thanks Rad.. unfortunately there's none such in my area. It's all Rite-Aids and CVS's round these parts. Any ideas where it can be gotten on the web?
You can also get it here:
http://www.chemistrystore.com/sodium_silicate.htm

Incidentally, that's also where I get sodium percarbonate for sanitizing my brewing supplies, and Propylene Glycol for the humidor.

But Rad's link looks WAY more fun! :twisted:
Kurt Huhn
AKA: Oversized Ostrogoth
artisan@k-huhn.com
User avatar
hazmat
Posts: 797
Joined: Thu Nov 23, 2006 8:00 pm
Location: Harrisburg, PA

Post by hazmat »

Good stuff. Thanks guys!
User avatar
KurtHuhn
Site Admin
Posts: 5326
Joined: Thu Nov 23, 2006 8:00 pm
Location: United States/Rhode Island

Post by KurtHuhn »

bvartist wrote:Out of curiosity.......why use pumice? I'm guessing it adds additional roughness to the coating when it is dried. Or is it something necessary in the waterglass recipe?
Yep. just an aid to make a rough surface for cake formation.
Kurt Huhn